Galvanized roof sheets are steel sheets dipped in molten zinc at the mill, then rolled into corrugated or IBR. The zinc rusts slowly in place of the steel, which is why a galvanised roof turns dull grey long before it shows red. It is the plain, lower cost sheet behind most farm sheds in the Free State, the old corrugated roofs in the Karoo and plenty of first roofs on backyard rooms. Whether you spell it galvanised or galvanized, the questions are the same: which zinc class, and does it suit the site.
Coating classes and what Z275 means
The coating is named by its mass: Z275 carries about 275 g/m² of zinc, both sides together, and is the common roofing class. Lighter classes such as Z200 or Z100 are cheaper and wear through sooner, and the thinnest yard sheets are often both light on zinc and light on steel. Ask for the class on the quote and on the delivery docket, with the thickness beside it; see roof sheet thickness. Some sheets show a spangle, a pattern of zinc crystals like frost on a window. Spangle is a look, not a measure of quality, and many modern sheets are made minimised or spangle free.
Where plain galvanised still makes sense
Inland, dry and clean air is where it does best: an implement shed near Bethlehem, a store on a Karoo farm, a workshop in Kimberley. It shortens fast in three places: near the sea, downwind of a factory or a mine stack, and over animals, where ammonia from poultry houses, piggeries and dairies attacks the zinc from below. For those sites look at aluminium zinc coated or painted sheets, or at fibre cement over the animals.
White rust on new sheets
New galvanised sheets stacked tight and left in the rain grow a white, powdery bloom between them. That is white rust: the zinc reacting with trapped water and no air. A light film brushes off and the sheet is fine; heavy, crusty bloom has eaten coating you paid for. Store sheets off the ground on bearers, tilted so water runs off, under cover, and fit them soon. Reject a delivery that arrives with thick white deposits.
Painting galvanised later
Bright new zinc does not hold paint well. Let it weather for some months or clean it with the treatment the paint maker gives, then use a primer meant for galvanised steel. On an old corrugated roof that is only dull and lightly rusted, painting can add years; once the sheets rust through along the purlins and laps, they are past painting and due for new sheets.
What to put in your request
- Say corrugated or IBR and the lengths
- Ask for the zinc class in writing
- Give the thickness, not just the price
- Say if animals will be housed under it
- Mention distance from the sea or a factory
Galvanised Roof Sheets: who asks for them and why
- Homeowners and DIY builders: a low cost roof on a backyard room, a garden store or a carport inland
- Roofers and roofing contractors: matching sheets for repairs to old galvanised corrugated roofs on farms and towns
- Builders, developers and quantity surveyors: plain sheets on site stores, temporary buildings and outbuildings off the main house
- Factories, warehouses and steel buildings: workshop and store roofs inland where the air is dry and free of fumes
- Shops, offices and business premises: covered parking or a yard store behind a business where looks matter less
- Farms: sheds, barns and animal houses: implement sheds, hay barns and stores, kept away from ammonia under animal houses
- Schools, churches, clinics and halls: sheds, bicycle shelters and stores on a school or municipal yard
- Landlords, body corporates and estate managers: storage and maintenance sheds where the estate rules allow a plain finish
Frequently asked questions
How long do galvanised roof sheets last?
Galvanised or Zincalume: which should I choose?
Can I mix new galvanised sheets with old ones?
Who will quote my galvanised sheets?
Work it out first
- Roof sheet calculatorEave length, slope and profile in, sheets, cut lengths and running metres out
- Roof pitch and area calculatorFootprint and pitch, or rise and run, in: slope length, sloped area and pitch out
- Purlin spacing calculatorProfile, thickness and roof or wall in: the typical span to check and purlins per slope